Skip to content
OKA-501 motor insulating lacquer
OKA-501 motor insulating lacquer, 4 L tinOKA-501 and Orchem products on a dealer shelf

OKA-501 Motor Insulating Lacquer (Class F, Air-Drying)

Class F (155 °C), very fast-drying air-drying lacquer for rewind shops. T-501, 4 L.

Technical information

Thermal classF (155 °C)
DryingAir-drying, very fast; no oven needed
Drying timeSee product TDS
BaseSee product TDS
ThinnerT-501
Thinning ratioTypically 3 varnish : 1 thinner
Packaging4 L tin
Best forRewind shops

Drying time, viscosity and pack sizes are given in the product TDS.

Air-drying varnishes

ProductBaseThermal classProperties and use
OR-100PhenolicB · 130 °CImpregnation of electric motors in small-batch production
OR-102PhenolicF · 155 °CFast-drying insulating varnish for rewind shops
OR-105High solidsF · 155 °CTransformer insulating varnish; applied by spray gun or dipping, thinned with T-100
OR-114 (2 BK 1024)2K polyurethaneH · 180 °CRoom-temperature curing motor insulating varnish; high chemical resistance, resistant to Freon and similar refrigerant gases
OKA-501See TDSF · 155 °CVery fast-drying insulating varnish, ideal for rewind shops. Thinned with T-501, 4 L tin

OKA-501 is a very fast-drying, air-drying class F (155 °C) motor insulating lacquer used to insulate electric motor windings. It needs no oven: it dries at ambient temperature and is thinned with T-501 thinner. Orhun Kimya makes it especially for rewind shops that rewind motors one by one and need to deliver them quickly.

As it dries on the finished winding, the lacquer forms an insulating film that protects the wire and winding against moisture, dust and dirt. Because it air-dries, you can treat the motor in the shop or on site without putting it in an oven.

Where is it used?

  • Electric motors rewound in motor repair shops,
  • Rewind jobs that must be delivered the same day or at short notice,
  • Shops without an oven, or parts that do not fit in one,
  • Electrical and electronic parts that need air-drying insulation.

Properties

  • Thermal class F (155 °C): in the IEC 60085 classification, F stands for 155 °C. It can be used on class F and lower-class (B, 130 °C) windings.
  • Very fast drying: cuts waiting time in the shop. Drying times are given in the product TDS.
  • No oven needed: dries at ambient temperature.
  • Thinner: T-501; typical ratio 3 parts varnish : 1 part thinner.
  • Packaging: 4 L tin.

How is it applied?

  1. Disconnect the motor. OKA-501 must not be applied to energized equipment.
  2. Clean dust, oil and old varnish residue from the winding. Dry a damp winding first; see the winding drying guide.
  3. Stir the tin thoroughly. If needed, thin only with T-501, usually 3 parts varnish to 1 part thinner.
  4. Apply the lacquer by a method suited to the part (dipping, brushing or spraying) so that it reaches the whole winding; let the excess drain.
  5. Leave the part to dry in a dust-free, well-ventilated place. Do not put the motor under load before the lacquer is fully dry.
  6. Close the tin tightly right after use.

Why and how much thinner is added is explained in the varnish thinning guide; all thinners are listed on the thinners page.

How to choose and what to watch for

If the winding is class F and fast turnaround matters, OKA-501 is a practical choice. If you prefer the phenolic OR 1xx series, see air-drying winding varnishes. For class H (180 °C) windings, the two-component OR-114 class H varnish, which cures without an oven, or baking winding varnishes if you have an oven, are better suited. The differences between classes are explained in the class B, F and H insulation guide.

For quick touch-ups on connections and terminals, motor insulating spray can also be used.

Common mistakes

  • Using another thinner: the right thinner for OKA-501 is T-501; a different one can spoil drying and film quality.
  • Over-thinning: the film gets thinner and insulation weaker.
  • Applying to a damp or oily winding: the lacquer does not bond and insulation resistance comes out low.
  • One thick coat: the surface dries while the layer beneath stays wet; two thin coats are better.
  • Running the motor before it is fully dry.

Safety and storage

OKA-501 is a solvent-containing lacquer thinned with thinner. Apply it in a well-ventilated place, keep it away from open flames and sparks, and wear gloves and safety glasses. Store the tin closed, in a cool, dry place out of direct sunlight. Shelf life and detailed safety information are given in the product TDS and safety data sheet.

For the OKA-501 technical data sheet (TDS), write to us via the form or WhatsApp.

Questions

What is OKA-501 used for?

OKA-501 insulates finished electric motor windings without an oven and protects them against moisture, dust and dirt. It is a very fast-drying, air-drying class F (155 °C) motor insulating lacquer.

What is OKA-501 thinned with?

OKA-501 is thinned with T-501 thinner; the typical ratio is 3 parts varnish to 1 part thinner. Do not use other thinners; the exact ratio is in the product TDS.

How long does OKA-501 take to dry?

OKA-501 is a very fast-drying lacquer; touch-dry and full-dry times are given in the product TDS, which you can request via the form or WhatsApp. Cold, humid conditions lengthen drying.

Does OKA-501 need an oven?

No. OKA-501 is air-drying and dries at ambient temperature.

What thermal class is OKA-501?

OKA-501 is class F (155 °C). It can be used on class F and B windings; for class H (180 °C) windings, OR-114 or baking varnishes are better suited.

What packaging does OKA-501 come in?

OKA-501 is supplied in 4 L tins.

Can OKA-501 be applied to a running motor?

No. OKA-501 must not be applied to energized equipment; disconnect the motor and clean and dry the winding first.

OKA-501 motor insulating lacquer, 4 L tinOKA-501 and Orchem products on a dealer shelfA rewinder working on a stator winding at the bench

More in this group

Related reading

Let's choose your varnish

Tell us the motor type, the operating temperature and how you apply varnish; we will send the right product, its TDS and a price.

+90 532 358 15 64
ali@orhunkimya.com.tr

Nothing you type is stored on our server; your message opens directly in WhatsApp or your email app.