| Type | 1K, solventless (100% solids) epoxy impregnating resin |
|---|---|
| Curing | Heat, latent anhydride cure system |
| Viscosity (25 °C) | 400–600 mPa·s |
| Density | 1.16–1.19 g/cm³ |
| Flash point | > 130 °C |
| Gel time | 15–30 min at 140 °C (5 g); 5–10 min at 165 °C |
| Application | Dipping, trickle, VPI |
Drying time, viscosity and pack sizes are given in the product TDS.
EPI-620 is a one-component, heat-curing epoxy resin for impregnating motor, generator and dry-type transformer windings. It contains no solvent (100% solids).
Where is it used?
- Impregnation of motor and generator windings,
- Dry-type transformer windings,
- Dipping, trickle and VPI (vacuum pressure impregnation) methods.
Why solventless?
With no solvent, volatility and shrinkage are reduced and voids during cure are less likely. Cure temperature and time are given in the TDS; test with your own oven profile before series production.
Questions
Does EPI-620 contain solvent?
No, it is a 100% solids system.
Which impregnation methods are suitable?
It is designed for dipping, trickle and VPI.
What is the cure schedule?
Cure temperature and time are given in the TDS; test with your own oven profile.