Skip to content
Insulating topcoat lacquers
Stator winding coated with red insulating topcoatWound rotors and commutators, close-up

Insulating Topcoat Lacquers and Paints (Anti-Flash): OR-990 and OR-411

Anti-flash topcoat: OR-990 (155–180 °C) and epoxy OR-411 (H); red, black, grey.

Technical information

OR-990One-component, solvent-based, air-drying insulating topcoat varnish
Thermal class range155–180 °C (IEC 60085)
AppearanceRed (oxide red) liquid; also made in black and grey
Density0.96–1.02 g/cm³ (23 °C, DIN 51757)
Flow time160–200 s, Ford 4 (25 °C)
Solids54–60 % (ISO 3251)
Drying (23 °C)Touch 20 min, slip 2 h, full 24 h
Drying (80 °C)Touch 5 min, slip 15 min, full 2 h
Dielectric strength> 140 kV/mm initial; > 100 kV/mm at 155/180 °C (IEC 60464-2)
Volume resistivity> 10¹⁶ Ω·cm initial; > 10¹¹ Ω·cm at 155/180 °C
Bond strength> 80 N (23 °C, IEC 61083)
ApplicationDipping or brushing; for spray gun add 10–20 % thinner by volume
Packaging400 ml spray, 1 L, 5 L, 20 kg
Shelf life24 months (23 °C, unopened)

Drying time, viscosity and pack sizes are given in the product TDS.

Anti-flash insulating topcoat paints

ProductBaseThermal classColour and production
OR-9901K, solvent-based155–180 °CAir-drying insulating topcoat varnish; red, black or grey
OR-411EpoxyH · 180 °CElectrical insulating topcoat paint; red, black or grey; made to order

Download the detailed TDS (PDF)

Summary values are in the table above. For the detailed TDS with all test methods, application and storage information, leave your name and email; the PDF downloads right away.

An insulating topcoat lacquer (anti-flash paint) is an insulating paint applied to the outer surface of motor, generator and transformer windings after the impregnating varnish has dried, adding a further layer of protection against moisture, dust, oil and surface tracking. Orhun Kimya makes two products in this group: the single-component, air-drying OR-990 and the epoxy-based class H OR-411.

Where is insulating topcoat used?

  • The outer surface and end windings of stator and rotor windings after varnishing,
  • Final protection of motors repaired in rewind shops,
  • Surface insulation of transformers and coils against moisture and contamination,
  • Touch-ups and small jobs (with the 400 ml OR-990 spray can).

A topcoat does not replace impregnating varnish: the varnish fills the inside of the winding, the topcoat seals the outside. When you need one is explained in the guide is an insulating topcoat necessary?

The difference between OR-990 and OR-411

OR-990 is a single-component, solvent-based, air-drying electrical insulating topcoat varnish. Its thermal class range is 155–180 °C (IEC 60085). At 23 °C it is touch-dry in 20 minutes and fully dry in 24 hours; at 80 °C full drying takes 2 hours. Initial dielectric strength is above 140 kV/mm. The standard colour is red (oxide red); black and grey are also made. It comes in 400 ml spray, 1 L, 5 L and 20 kg packs.

OR-411 is an epoxy-based class H (180 °C) electrical insulating topcoat paint, made to order in red, black or grey. Epoxy coatings generally offer good resistance to chemicals and abrasion. The mixing, application and curing conditions of OR-411 are given in its TDS.

Properties

  • Forms a glossy, sealed surface over the varnished winding,
  • Gives extra protection against moisture and water,
  • Reduces dust and oil build-up and makes the winding easier to clean,
  • Adds one more layer against mechanical impact and abrasion,
  • Being coloured, it shows at a glance during maintenance whether the winding is coated.

How is it applied?

  1. Make sure the impregnating varnish is fully dry or cured.
  2. Clean dust, oil and varnish runs from the surface.
  3. Stir OR-990 well before use; apply by dipping or brushing.
  4. For spray-gun application add 10–20 % thinner by volume; the right thinner is stated in the product TDS.
  5. Apply a thin, even coat; if needed, apply a second coat once the first is dry.
  6. Wait 24 hours at 23 °C or dry for 2 hours at 80 °C, then put the motor into service.

For OR-411, follow the mixing, application and curing instructions in its TDS.

How to choose

For general rewind and maintenance work, single-component, fast-drying OR-990 is practical. Consider OR-411 where class H (180 °C) and epoxy resistance are required. The topcoat should match the thermal class of the varnish beneath: on a winding treated with class H baking varnish or OR-114, the topcoat must also meet that class. See the thermal class guide. For impregnation, see our air-drying winding varnishes; for small on-site jobs, the motor insulating spray.

Common mistakes

  • Topcoating over varnish that is not dry: trapped solvent can blister the surface or leave it soft.
  • Using only a topcoat instead of impregnation: the inside of the winding stays uninsulated.
  • One very thick coat: drying takes longer and the paint runs.
  • Too much or the wrong thinner for spraying: the film gets thin and drying suffers.

For the OR-990 and OR-411 TDS, write to us via the form or WhatsApp.

Questions

What does an insulating topcoat lacquer do?

It seals the outer surface of a varnished winding, adding protection against moisture, dust, oil and surface tracking. It is applied over the impregnating varnish, not instead of it.

What does anti-flash paint mean?

Anti-flash is the name used for insulating topcoat paints that protect the winding surface against tracking and flashover caused by moisture and dirt. OR-990 and OR-411 belong to this group.

How long does OR-990 take to dry?

At 23 °C it is touch-dry in 20 minutes, slip-dry in 2 hours and fully dry in 24 hours. At 80 °C full drying takes 2 hours.

What is OR-990 thinned with?

It is used as supplied for dipping and brushing; for spray guns 10–20 % thinner by volume is added. The right thinner is stated in the product TDS; request it via the form or WhatsApp.

What is the difference between OR-990 and OR-411?

OR-990 is single-component, solvent-based and air-drying, with a thermal class range of 155–180 °C. OR-411 is an epoxy-based class H (180 °C) topcoat paint made to order; its curing conditions are in its TDS.

What colours are available?

OR-990 is standard red (oxide red) and is also made in black and grey. OR-411 is made in red, black or grey.

Is the insulating topcoat available as a spray?

Yes. OR-990 also comes in a 400 ml spray can, besides 1 L, 5 L and 20 kg packs.

Stator winding coated with red insulating topcoatWound rotors and commutators, close-upA rewinder working on a stator winding at the bench

More in this group

Related reading

Let's choose your varnish

Tell us the motor type, the operating temperature and how you apply varnish; we will send the right product, its TDS and a price.

+90 532 358 15 64
ali@orhunkimya.com.tr

Nothing you type is stored on our server; your message opens directly in WhatsApp or your email app.