OR-3200 GC Glass-Fibre Conductor Varnish
Varnish for glass-fibre covered conductors; thinned with T-3200.
Technical information
| Product code | OR-3200 GC |
|---|---|
| Application | Glass-fibre covered flat and round conductors |
| Appearance | Clear liquid |
| Solids | 48–50% (IEC 60851-2) |
| Viscosity | DIN 4, 25 °C: 14–18 s |
| Density | 0.96–0.98 g/cm³ |
| Gel time | 8–10 min at 170 °C |
| Dielectric strength | ≥15 kV/mm (after cure) |
| Thinner | T-3200 thinner |
| Pack | 16 and 200 kg metal drums |
| Shelf life | At least 3 months, store at 5–25 °C |
Drying time, viscosity and pack sizes are given in the product TDS.
OR-3200 GC is a varnish developed for insulating glass-fibre covered flat and round conductors. Viscosity is adjusted with T-3200 thinner.
Highlights
- Clear liquid with low viscosity,
- Dielectric strength of ≥15 kV/mm after cure (typical 18–22 kV/mm),
- Detailed test results are given in the TDS.
Thinning
Use T-3200 thinner for viscosity adjustment and equipment cleaning. Use within 24 hours after mixing.
Questions
Which conductors is it for?
It is designed for glass-fibre covered flat and round conductors.
Which thinner is used?
T-3200 thinner. Use within 24 hours after mixing.
What is the shelf life?
At least 3 months when stored at 5–25 °C.